Formulyte

Electrolyte formulation and testing

Custom electrolytes for battery research.

We mix electrolytes to the composition you specify, then measure what they do. Lithium and sodium systems in research quantities, including blends that no supplier keeps in stock.

Services

What we do

Most suppliers sell from a fixed catalogue and ship a certificate of analysis. We work from your specification instead, and the measurements come with the bottle.

Custom formulation

You give us the salt, the solvent ratio and the additives. We prepare it under argon and send it with a sheet listing exactly what went in.

Electrochemical testing

Ionic conductivity across a temperature range, impedance spectroscopy, and coin cell cycling. You get the data files, not only a summary table.

Incoming material checks

Salts and solvents are tested for water and free acid before we use them. Every lot has a recorded result, and we will show it to you.

Handling

Most of the contamination happens after the bottle

Electrolyte testing usually runs on repeated pipetting, open vials and manual transfers. Even inside an argon glovebox, solvent evaporates off an open tip, trace moisture finds its way in, and pipetted volumes drift between batches. Those shifts change the interphase that forms, which changes cycle life, which changes the conclusion you draw.

01

Closed transfer

The liquid is not exposed to the glovebox atmosphere or to shared tools between leaving its container and reaching the cell.

02

Fixed dose

Volumes are delivered at a set amount rather than pipetted by hand, so the dose does not drift from one cell to the next across a batch.

03

One path per formulation

Each formulation gets its own single-use fluid path, so nothing carries over from the composition before it.

04

Water held to the end

The ppm figure on the certificate is meant to be the figure when the cell is sealed, not the figure when the bottle was filled.

This matters most where the chemistry is delicate: SEI-forming additives, high-voltage cathodes, sodium systems. Your cycling data should describe the electrolyte you chose, not the handling it went through on the way in.

In the lab

What we can measure

01

Argon glovebox

Mixing and handling are done under argon. Water is kept low enough that the salts do not start breaking down before the experiment does.

02

Impedance spectroscopy

EIS across frequency and temperature. Cell constants are measured against a KCl standard rather than taken from the manufacturer's sheet.

03

Ionic conductivity

Conductivity measured over a temperature range, with the Arrhenius fit reported where the data supports one.

04

Coin cells

We build and cycle 2032 coin cells so that two electrolytes can be compared on the same electrodes and the same schedule.

05

Lithium and sodium

LiPF6, LiFSI and LiTFSI, the sodium equivalents, and ionic liquid based systems as well as carbonates.

06

Written records

Each batch leaves with its composition, its water content and whatever properties we measured, on paper.

Background

Why the electrolyte matters

It decides how fast a cell can charge, how cold it can run, and what layer forms on the electrodes during the first cycles. Most groups buy it from a catalogue and then work around whatever they were sent.

20–30
per cent
of lithium-ion cell manufacturing cost goes to formation and ageing, the stage where the electrolyte builds the interphase.
1.5–3
weeks
is a normal formation time for a lithium-ion cell, limited by how quickly a stable interphase can be grown.
<20
ppm water
is the level an electrolyte has to hold before any of the numbers above can be trusted.

Figures above are from published work on lithium-ion cell manufacturing. They are not Formulyte measurements.

How we work

Small batches, written down properly

We are a small lab. That sets what we can take on, and it is also why the record keeping is tight.

Every batch is measured

Nothing ships on the assumption that it came out right. You get the measurement and the file it came from.

Research quantities

Orders start at the scale an experiment actually needs. There is no 500 gram minimum.

Failed runs are reported

If a measurement does not reproduce, it goes in the report that way instead of being quietly dropped.

Contact

Send us a composition

Tell us the chemistry, how much you need, and what you want measured. We will come back with a price and a date.

We work with university research groups, battery startups and industrial R&D teams, on custom formulations and on the handling protocol around them.

contact@formulyte.com
Location
Montréal, Québec
Chemistries
Li-ion and Na-ion
Status
Taking early enquiries